◆Polycrystalline infrared fiber for the mid-infrared wavelength range of 3~17μm ◆Low loss of 0.2dB/m at 9~13μm ◆High temperature resistance (up to 410°) ◆Free of harmful substances
●CO2 laser transmission possible up to 40W
【Specifications】
Core/Clad Structure: AgCl:AgBr
Spectral Range: 3 – 17 μm
Core Refractive Index: 2.15
Fresnel Reflection Losses for two surfaces: 25%
Attenuation at 10.6 µm: 0.2 – 0.4 dB/m
Numerical Aperture NA: 0.3 +/- 0.03
Melting Point: 410 °C
Operating Temperature: –273 to +140°C
Core/Clad Diameter (standard): see Parameters of standard Polycrystalline fibers
Laser Damage Threshold for CW CO2 laser: >12 kW/cm²
Tensile Strength: > 70 MPa
Minimum Bending Radius (fixed): 5 x [Fiber Diameter]
Minimum Elastic Bending Radius: 150 x [Fiber Diameter]